CPE 135B
1.Properties
It is a kind of amorphous elastomer with minimal crystal. It has lower Mooney viscosity and mastication
temperature as well as excellent properties such as good processing property, excellent weathering
resistance, good flex resistance and flame resistance. It can be blended with CR, CSM, NBR, EPDM,
SBR and NRat any ratio.
2.Specifications
We have all whole series CPE 135B products lines, like CM3645, CM3650 and CM3675 etc.
Technical data and just reference feed rate:
Items | Unit | Specification |
Chlorine Content | % | 35-37 |
Heat of Fusion | J/g | ≤1.5 |
Shore Hardness | Shore A | ≤55 |
Tensile Strength | Mpa | ≥8.0 |
Elongation at Break | % | ≥700 |
Mooney Viscosity | ML(1+4)125℃ | 70-80 |
Impurity Particles | Particles/100g | ≤20 |
Stable Time(165℃) | Min | ≥8 |
Volatile Matter | % | ≤0.3 |
3.Uses
It can be used as special synthetic rubber, as well as modifier or solubilizing agent of general purpose synthetic rubber.
CPE 135B+cross-linking agent + toher additives: Manufacture various flame-retardant wire and cable sheath, seals.
CPE 135B+CR+cross-linking agent + other additives: Manufacture various flame-retardant wire and sheath, hose, sheeting, seals.
CPE 135B+ EPDM+ flame retarder+cross-linking agent + other additives: Manufacture various oil resistant
wire and cable restardant wire and vable insulaton, waterproof sheeting, automobile weather strip. The above rubber can be processed by common equipment and technology in rubber industry.
4.Package
Packed in plastic weaved bag,lined with a PE bag, 25kg in weight. It can be stored in a cool dry place with goodventilation. The expiring date is 12 months from the date o produced, but can be used if passed in